Abstract

This paper is focused on cobalt valorization from the cathode material of spent lithium-ion batteries (LIBs) by using leaching and electrochemical deposition methods. During the leaching experiments, the degrees of cathode material dissolution in H2SO4-N2 and H2SO4-O2 systems were compared. Maximal degrees of cobalt extraction were 40 % in the former and 47 % in the latter system under following experimental conditions: H2SO4 concentration of 2 mol dm-3, nitrogen/oxygen volumetric flow of 2 L min-1, solid phase concentration of 33 g L-1, and temperature of 85?C. The rate of cobalt extraction from the cathode material in both investigated systems was the most favorable in the first 15 min, after which there was a sudden decrease in the reaction rate. Cobalt from the leaching solution was deposited on a copper substrate by galvanostatic electrochemical deposition with a current efficiency of 84%. The energy consumption was 5.8 kWh kg-1 of deposited Co. The cyclic voltammetry (CV) method was used to determine the potential of cobalt deposition, as well as side reactions taking place in the system. Scanning electron microscopy with energy dispersive spectrometry has shown that during the process of electrochemical deposition agglomeration of cobalt particles occurred (in the shape of cauliflower), while the metal was deposited in its elemental state, which was also confirmed by the results of X-ray diffraction analysis.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.