Abstract

The Ce0.5Zr0.4Co0.1O2/Pd-Al2O3 composite prepared by a mechanochemical route with high BET surface area of 33 m2 g−1, exhibited the high oxygen storage capacity (OSC), and high CO oxidation activity at the low temperatures even after calcination at 1000°C for 20 h.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.