The total cobalt and nickel concentration of 11 brands of Asian cement ranged from 8.1 to 14.2 micrograms/g and 14.9 to 28.5 micrograms/g, respectively. These metals exist mainly as insoluble salts; the water-soluble concentration of cobalt and nickel in the cements ranged from 0.39 to 0.65 micrograms/g and from 0-1.2 micrograms/g, respectively. 1.5% (4/272) of construction workers in a prefabrication construction factory had cobalt sensitivity. All had allergic contact dermatitis from chromate in cement. No worker had isolated cobalt sensitivity and cement dermatitis. It appeared that sensitization to cobalt in cement occurs only secondarily to an existing cement dermatitis. 1.8% (5/272) workers had nickel sensitivity: 2 with allergic contact dermatitis to nickel in their watches, 2 were asymptomatic and 1 had allergic contact dermatitis to chromate and cobalt in cement. The low prevalence of cobalt and nickel sensitivity from cement was probably related to the low concentration of soluble cobalt and nickel salts in the cement. However, these insoluble salts can form soluble complexes with body fluids on eczematous skin and sensitize the skin.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.