Abstract
This paper experimentally investigates the cut quality of laser cutting for the age hardened Inconel 718 nickel based super alloy, with the use of a continuous CO2 4.0kW laser cutting system. The quality of the cut has been monitored by measuring the kerf taper ratio, the recast layer thickness and the surface roughness of the cut specimens. The effects of processing parameters, such as the laser power, the cutting speed and the assisting gas pressure were evaluated. Scanning electron microscopy (SEM), Energy Dispersive Spectrography (EDS), X–Ray Diffraction (XRD), Atomic Force Microscopy (AFM) and Knoop hardness tests are carried out to examine the cutting defects, the kerf size variation and formed carbide on the surfaces. A statistical analysis of the results has been performed in order for the effect of each parameter on the cutting quality to be determined. The regression analysis has been used for the development of empirical models able to describe the effect of the process parameters on the quality of laser cutting.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.