Abstract

The objectives were to compare the duration of use of polymeric tracheostomy tubes, i.e., silicone (Si), polyvinyl chloride (PVC), and polyurethane (PU), and to determine whether surface changes in the materials could be observed after 30 days of patient use. Data were collected from patient and technical records for all tracheostomized patients attending the National Respiratory Center in Sweden. In the surface study, 19 patients with long-term tracheostomy were included: six with Bivona TTS Si tubes, eight with Shiley PVC tubes, and five with Trachoe Twist PU tubes. All tubes were exposed in the trachea for 30 days before being analyzed by scanning electron microscopy (SEM) and attenuated total reflectance Fourier transform infrared spectroscopy (ATR-FTIR). New tubes and tubes exposed in phosphate-buffered saline were used as reference. Si tubes are used for longer periods of time than those made of PVC (P<.0001) and PU (P=.021). In general, all polymeric tubes were used longer than the recommended 30-day period. Eighteen of the 19 tubes exposed in patients demonstrated, in one or more areas of the tube, evident surface changes. The morphologic changes identified by SEM correlate well with the results obtained by ATR-FTIR. Si tracheostomy tubes are in general used longer than those made of PVC and PU. Most of the tubes exposed in the trachea for 30 days suffered evident surface changes, with degradation of the polymeric chains as a result.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call