Recent efforts to improve the interface between implant and bone have involved the use of bioactive materials, specifically hydroxyapatite (HA). HA coatings applied to implants have shown excellent clinical results at 2 years. There have been no radiolucent lines around the HA-coated implants. The long-term strength of the HA coating-substrate bone interface remains a concern as osseointegration of the HA appears to be a consistent phenomenon. This can lead potentially to an interruption between the substrate itself and the osseointegrated coating.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.