Abstract

Cobalt is a critical resource in industrial economies for the manufacture of electric-vehicle batteries, alloys, magnets, and catalysts, but has acute supply-chain risks and poses a threat to the environment. Large-scale sequestration of cobalt in low-cost materials under mild conditions opens a path to cobalt recycling, recovery and environmental clean-up. We describe such sequestration of cobalt by a widely available commercial calcium silicate material containing the mineral xonotlite. Xonotlite rapidly and spontaneously takes up 40 percent of its weight of cobalt under ambient conditions of temperature and pressure and reduces dissolved cobalt concentrations to low parts per million. A new Sharp Front experimental design is used to obtain kinetic and chemical information. Sequestration occurs by a coupled dissolution-precipitation replacement mechanism. The cobalt silicate reaction product is largely amorphous but has phyllosilicate features.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call