Abstract
Despite wide resection and systemic chemotherapy, bone tumors may present with local recurrences, metastases and pathological fractures. Application of bone cement containing antineoplastic drug to fill the defect after resection of metastatic lesions and to support implants has been suggested to prevent local tumor growth and implant failures. In this study, we aimed to demonstrate the effects of the addition of cisplatin which is a widely used antineoplastic drug for osteosarcoma, on the mechanical properties of bone cement, and to evaluate the cytotoxic effects of eluted cisplatin on Saos-2 cell culture. Two cement samples were prepared by mixing 100 mg and 300 mg of cisplatin powder with 40 g cement powder. The bone cement of the control group did not contain cisplatin. Mechanical analyses included 4-point bending, compression and shear testing. For cytotoxicity analysis, samples were incubated in Dulbecco's Modified Eagle's medium for 15 days. Mediums were applied to Saos-2 cell culture and cell viability was measured. Surface analyses were performed by scanning electron microscope (SEM). The addition of cisplatin did not alter the mechanical properties of bone cement. It was observed that the eluted cisplatin had cytotoxic effects on Saos-2 cells. SEM analyses demonstrated cisplatin granules on the surface of cement samples. Cisplatin maintains its cytotoxic property when released from bone cement without compromising the mechanical stability. Application of cisplatin loaded bone cement may help local control of tumor growth. We believe that our study will shed light on to these new practices for the treatment of bone cancers and will encourage future studies.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.