Abstract

Chromatic dispersion in the 1.47-1.60 μm wavelength region is measured successfully for a dispersion-shifted fibre over 120 km by the LD phase-shift method. The measured value of a 123 km spliced fibre agrees well with the sum of chromatic dispersion values of its constituent fibres. This confirms the additive rule of chromatic dispersion for long dispersion shifted fibre in the 1.5 μm wavelength region.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.