Abstract

Transition from passive state to stable localised corrosion of reinforcement steel in concrete owing to chloride ingress takes place over a period of time rather than being a one-step-occurrence. The depassivation process was characterised by frequent measurements of corrosion potential, polarisation resistance, and macro-cell currents when short-circuiting the working electrode with additional cathode surface. In addition, the concrete resistivity was continuously monitored and cathodic and anodic polarisation curves were measured. The results are consistent and imply that the localised corrosion process is in the initial phase of pit growth under mixed anodic/ohmic control. With time, the anodic reaction kinetics become more limited and the corrosion rate gets almost entirely determined by anodic control. The observed relationship between achieved maximum corrosion current and concrete resistivity indicates that the extent to which the anodic reaction kinetics are restricted is determined by the concrete microstructure and its ability to retain ionic movement.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.