Abstract

AbstractCa20Al26Mg3Si3O68 :xCe3+,yDy3+ (x = 0.02‐0.12; y = 0‐0.09) phosphors are prepared by solid state reaction of CaCO3, Al2O3, MgO, SiO2, Li2CO3 (as charge compensator for the lanthanoide dopants), CeO2, and Dy2O3 in stoichiometric amounts (corundum crucible, 5% H2/N2, 1400 °C, 2 h).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.