Abstract
AbstractReview: 73 refs.
Full Text
Sign-in/Register to access full text options
Published version (
Free)
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
https://doi.org/10.1002/chin.201616205
Journal: ChemInform | Publication Date: Mar 1, 2016 |