Abstract

AbstractThe synthesis methods of ZrB2 powders using ZrO2 + B2O3 + C (carbothermal reduction), ZrO2 + B4C (boron carbide reduction), and ZrO2 + B4C + C (combined reduction) at 1250 °C for 1—3 h under flowing Ar are compared.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.