Abstract

AbstractCrystals of KCdCO3F (I), RbCdCO3F (II), KZnCO3F (III), and RbZnCO3F (IV) are grown under subcritical hydrothermal conditions, using e.g. a 1:6:2 molar mixture of CdCl2, KF, and K2CO3 in H2O for KCdCO3F (autoclave, 220 °C, 5 d).