AbstractBiNbO4 (I) and BiTaO4 (II) powders are obtained via the sol‐gel citrate route, starting with 5% excess of Bi(NO3)3 in aqueous solutions of niobium or tantalum citrate peroxide (pH 7—8, solvent evaporation at 180 °C, 4 h, calcination at 550—1200 °C, 3 h).