AbstractKMSO4F (M: Fe, Co, Ni) is prepared by ball milling of equimolar mixtures of KF and MSO4 for one hour followed by heating (Parr reactor, 270—290 °C, 40—45 h).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.