Abstract

AbstractThe title mixed‐phase oxide catalysts for NO oxidation in diesel exhaust are prepared by co‐precipitation from an aqueous mixture containing Mn(OAc)2, Sr(NO3)2, Ce(NO3)3, Sm(NO3)3, Gd(NO3)3, (NMe4)OH, oxalic acid, and H2O2 (pH 9—10) followed by calcination at 500 °C and 800 °C for 8 h each.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.