Abstract

Chemical vapor deposition of TiN on Si wafers is carried out in a cold wall reactor at pressures in the range 100-300 mtorr and temp. between 450 °C and 700 °C using TiCl4 and NH3 as reactants.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.