Boron doped zinc oxide films were deposited by atmospheric pressure chemical vapor deposition in a laminar flow reactor from diethyl zinc, tert-butanol, and diborane in the temperature range from 300 to 420 o C. When the deposition temperature was above 320 o C, both doped and undoped films have highly oriented crystallites with their c-axes perpendicular to the substrate plane

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.