Abstract

AbstractSingle crystals of the title compound are obtained by heating a mixture of Tl2WO4, WO3, and Sm2O3 to 900 °C (5:2:1, Pt crucible, 24 h; the excess tungstate is used as a flux).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.