Abstract

AbstractPure and Nd‐doped Ca9La(VO4)7 crystals with various Nd3+ levels (3.2, 18.9, 31.4, and 32 at.%) are grown by the Czochralski method at 1430 °C from powders prepared by solid state reaction of a stoichiometric mixture of CaCO3, V2O5, La2O3, and Nd2O3 (alumina crucible, 1000 °C, 8 h).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.