Abstract

AbstractPolycrystalline samples of Sr2BIrO6 (B: In, Sc, Fe, Co, Ti) are prepared from citrate precursors using stoichiometric mixtures of Sr(NO3)2, IrO2, In2O3, Sc2O3, FeC2O4, Co(NO3)2, and TiC10H14O5 in aqueous solutions of citric acid and HNO3 followed by heating of the resulting resins (600 °C, 12 h) and calcination in air (1100—1200 °C, 12 h).