AbstractPolycrystalline 10H‐BaFeCl0.13O2.48 is prepared as a single phase by sintering a 1.87:1:0.13 molar mixture of BaCO3, α‐Fe2O3, and BaCl2 (Al2O3 crucible, 850 °C, 2 d) followed by grinding and reheating (800 °C, 3 d) and two further heat treatments (820 and 900 °C, 1 d each).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.