Abstract

AbstractThe misfit layered mixed oxide Ca3Co4O9 is prepared by calcining a mixture of CaCO3 and Co2O3 (850 and 900 °C, 1 d each) followed by epicyclic milling and final sintering in O2 (Pt crucible, 940 °C, 100 h).