Abstract

In this communication, we report a facile strategy to chemically synthesize anisotropic SmCo5 nanomagnets with a large magnetic energy product (BH). First, we designed a Co3O4@Sm2O3-CaO precursor by a one-pot method, which could be further reduced into uniform single-crystal SmCo5 particles under the stabilization of CaO coating. Following that, CaO was removed under an oxygen-free environment to impede oxidation. Finally, 130 ± 10 nm SmCo5 particles were aligned to be nanomagnet, exhibiting a large (BH)max value of 18.1 MGOe, which is the highest value reported by chemical methods.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.