Abstract
The Al filming of steel using the disproportionation of Al subsulphide was studied. Chemical vapour deposition was realised using (2Al2O3+6C+Al2S3) or (4Al+Al2S3) as reaction mixture at 1100°C and pressure of 5 Pa. It is indicated that the coating formed by evaporation of (2Al2O3+6C+Al2S3) consists of α-Fe and Al13Fe4, possesses thin diffusion layer and dark rough surface and is resistant to solution of nitric acid with alcohol, but the coating formed by evaporation of (4Al+Al2S3) consists of Fe3Al and AlFe and possesses thick diffusion layer and bright smooth surface.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: Materials Technology
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.