Abstract

Oxide chemical analysis of White Tower samples showed that the major oxides (content > 5%) are, %: SiO2–50.07; Al2O3– 16.3; Fe2O3– 7.04; CaO – 9.08. The loss on ignition is 11.32. In addition, elemental analysis determined a heightened carbon content carbon – 9.59%. The heightened carbon content (9.59%) in the inclusions attests the introduction of fuel into the green body, which increases the porosity of the articles and promotes uniform sintering of the ceramic, and the heightened content of alkali oxides (R2O > 3 – 4%) promotes the formation of a glass phase up to 1000°C. X-ray phase analysis showed the presence of anorthite, hematite, and wollastonite, which promotes greater strengthening. Moreover, the presence of isometric pores and oval closed porosity in the ceramic samples increases durability.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.