Abstract
Desulfurization and demineralization by an aqueous caustic leaching method was investigated of an asphaltite sample from Harbul (Silopi, SE Anatolia, Turkey). The effects of different parameters, such as alkali concentration, time, and temperature, on the leaching efficiency were detailed and the experimental results are presented here. The caustic concentration varied from 0.1–1.0 M, temperature was 100–180°C, and leaching time varied from 4–16 h. The removal of total sulfur and ash increases with increasing alkali concentration, leaching temperature, and time. As a result of aqueous caustic leaching, the ash content of asphaltite was reduced from 32.49 to 18.00%, and 76% of combustible was recovered. Total sulfur and volatile matter content was reduced from 7.02 to 2.68% and from 46.74 to 25.10%, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Energy Sources, Part A: Recovery, Utilization, and Environmental Effects
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.