Abstract
In this article, we studied the anelastic properties at low-load nanoindentations of different metallic glasses, including Zr-, Pd-, La-, Mg-, and Au-bases. It is verified that the “two-parameter Kelvin model” is suitable for analyzing the anelastic mechanical behavior. Despite the difference in the chemical composition of these alloys, the energy barrier against the local relaxation is almost equal. The energy barrier is much smaller than that of slow β relaxation, which denotes a faster relaxation mechanism. These findings give insights into the heterogeneous nature of mechanical behavior and relaxation characteristics of metallic glasses.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.