Abstract

The objective of this study was to use Raman spectroscopy to study the morphology and chemical changes of alkali–silicate reaction (ASR) products over time. The reaction products induced by ASR on soda-lime glass slides in a high temperature alkaline environment (1 N NaOH at 80 °C) enriched with calcium hydroxide were studied at 0, 1, 4, 7, 14 and 28 days. The results show that the morphology of the granular-like and fan-like fascicles structure that formed at early ages was more ordered in terms of polymerization and dominated by Q3 and Q2 units. This information implies that the ASR products were probably of mainly alkali silica composition with low content of calcium in the structure. As the reaction proceeded the products depolymerized, forming a cloud-like morphology of decreased structural order which surrounded the initial product particles. It can be hypothesized that more calcium ions in the soak solution entered into the particle structure, promoting a depolymerization and possible formation of a C–S–H phase which was indicated by the dominant presence of Q1 units after 7 days of exposure. To corroborate the interpretation of Raman spectra, 28-day ASR products were verified by Fourier transform infrared.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.