Abstract
Two Turkish lignites (Beypazari and Tunçbilek) were leached with the solutions of hydrogen peroxide in water or in 0.1 N H 2SO 4. The effects of some process parameters, such as concentration, time and temperature, on the removal of ash and sulphur have been investigated. The rate of ash and sulphur removal are relatively high in the first 30 min, but slow after 60 min of the reaction time. Depending on the type of lignite, the maximum reductions ranged from 30 to 70% in ash, from 70 to 95% in pyritic sulphur, and from 42 to 58% in total sulphur. A relatively small reduction (a maximum of 25%) was estimated for organic sulphur. The optimum process conditions were established as a hydrogen peroxide concentration of 15 wt.%, a temperature of 30 °C and a leaching time of 60 min. High peroxide concentration or high temperature did not result in an appreciable further reduction in ash and sulphur. Due to partial dissolution or oxidation of the lignites, some organic material losses occurred but no heating value loss was estimated. An overall kinetic approach was also applied for pyritic sulphur removal, and the conversion data were analyzed by using both homogenous and heterogeneous reaction models.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.