Abstract

During the thermal decomposition of orthorhombic ammonium perchlorate (AP) at 230°C, where the decomposition is only up to 30 wt %, there is an accumulation in the solid of acids, the concentration of which increases up to 15% decomposition, after which it decreases till it reaches the original value. Similar observations have been made in the polystyrene (PS)/AP propellant systems. Aging studies of PS/AP propellants have been carried out earlier [1], where it has been shown that for the aged propellants the thermal decomposition (TD) rate at 230°C and 260°C and ambient pressure burning rate ( r ̇ ) both increase and this increase is due to the formation of reactive intermediate “polystyrene peroxide (PSP).” In the present studies it has been observed that during the aging of the propellant at 150°C, the acid is formed and gets accumulated in the propellant, which may also be responsible for the increase in TD rate and perhaps may be more effective than PSP.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.