Abstract

Rare earth-iron magnetostriction alloy (0.1g) was decomposed with hydrochloric acid and hydrogen peroxide within a few minutes. The solution obtained was diluted to 100ml with water. To 10 ml of this diluted solution, an internal standard solution and hydrochloric acid were added and then diluted to 100 ml again with water. The amounts of Mn, Fe, Tb and Dy were measured by ICP-AES without any concomitant effect. Among the internal standard elements investigated (Sc, Y and La), La was most suitable. Recoveries of each element measured with a synthetic sample solution were over 99.7%. The relative standard deviations (n=5) were 0.04%0.35%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.