Abstract
Solid state 7Li and 19F magic angle spinning nuclear magnetic resonance (MAS NMR) experiments are conducted on several cathodes containing CFx–Silver vanadium oxide (CFx–Ag2V4O11) hybrid cathodes discharged to 50% depth of discharge (DoD) and stored at their open-circuit voltage for a period of one and three months. Three carbonaceous sources for the CFx phase are investigated: petroleum coke-based, fibrous, and mixed fibrous. For each hybrid cathode, a measurable increase in the relative amount of lithium fluoride is observed after a three month resting period in both the 7Li and 19F NMR spectra. These changes are attributed to lithium ion migration from the silver vanadium oxide to the CFx phase during the resting period, and help clarify the mechanism behind high power handling capability of this cathode.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.