Abstract

Nickel sulfide (NiS) as a cathode material for a lithium rechargeable battery was charged and discharged at elevated temperature (80 °C) using a PEO solid polymer electrolyte. In order to synthesize a homogeneous NiS phase, very fine nickel metal powder was ball milled with sulfur powder for 12 h under argon gas. We found using ex-situ XRD measurements that the NiS cathode active material was transformed into other phases such as Ni 3S 2, nickel and sulfur during discharge. The initial discharge capacity of the NiS positive electrode was 580 mAh/g NiS at 1.5 V vs. Li/Li + with PEO electrolyte. It has good cycling properties, retaining 93% of the initial discharge capacity even after 200 cycles with a PEO solid polymer electrolyte.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.