The WO 3 -Nb 2 O 5 electrochromic films were deposited by bipolar pulsed magnetron sputtering. The optical-density of WO 3 -Nb 2 O 5 film was a closer to WO 3 film. The response-speed and duration were increased by Nb 2 O 5 doped WO 3 films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.