Abstract

W–20Cu ultrafine composite powder, whose average grain size was about 500 nm, was fabricated by spray drying and calcining-continuous reduction technology. In the W–20Cu ultrafine powder the nanocrystalline Cu grain can wet W grain by the CuO transitional layer, the special non-metal–metal nanocomposite structure would play very important roles in obtaining W–Cu alloy with good mechanical properties, thermal conductivity and homogeneous microstructure.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.