Abstract
New data of creep and viscoelastic Poisson’s ratio, , of five engineering elastomers (Ethylene Propylene-Diene Monomer, Flouroelastomer (Viton®), nitrile butadiene rubber, silicone rubber and neoprene/chloroprene rubber) at different stress (200, 400 and 600 kPa) and temperature (25, 50 and 80 °C) are presented. The was characterized through an experimental methodological approach based on creep testing (30 min) and strain (axial and transverse) measurements by digital image correlation. Initially, creep behavior in axial and transverse directions was characterized for each elastomer and condition, and then each creep curve was fitted to a four-element creep model to obtain the corresponding functions. The obtained functions were used to estimate for prolonged times (300 h) through a convolution equation. Overall, the characterization was achieved for the five elastomers results exhibiting increasing with temperature and time from about 0.3 (for short-term loading) to reach and stabilize at about 0.48 (for long-term loading).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.