Abstract
Solid-state lithium-metal (Li0) batteries are gaining traction for electric vehicle applications because they replace flammable liquid electrolytes with a safer, solid-form electrolyte that also offers higher energy density and better resistance against Li dendrite formation. Solid polymer electrolytes (SPEs) are highly promising candidates because of their tuneable mechanical properties and easy manufacturability; however, their electrochemical instability against lithium-metal (Li0), mediocre conductivity and poorly understood Li0/SPE interphases have prevented extensive application in real batteries. In particular, the origin of the low Coulombic efficiency (CE) associated with SPEs remains elusive, as the debate continues as to whether it originates from unfavoured interfacial reactions or lithium dendritic growth and dead lithium formation. In this work, we use state-of-the-art cryo-EM imaging and spectroscopic techniques to characterize the structure and chemistry of the interface between Li0 and a polyacrylate-based SPE. Contradicting the conventional knowledge, we find that no protective interphase forms, owing to the sustained reactions between deposited Li dendrites and polyacrylic backbones and succinonitrile plasticizer. Due to the reaction-induced volume change, large amounts of cracks form inside the Li dendrites with a stress-corrosion-cracking behaviour, indicating that Li0 cannot be passivated in this SPE system. On the basis of this observation, we then introduce additive engineering, leveraging from knowledge of liquid electrolytes, and demonstrate that the Li0 surface can be effectively protected against corrosion using fluoroethylene carbonate, leading to densely packed Li0 domes with conformal and stable solid-electrolyte interphase films. Owing to the high room-temperature ionic conductivity of 1.01 mS cm-1, the high transference number of 0.57 and the stabilized lithium-electrolyte interface, this improved SPE delivers an excellent lithium plating/stripping CE of 99% and 1,800 hours of stable cycling in Li||Li symmetric cells (0.2 mA cm-2, 1 mAh cm-2). This improved cathodic stability, along with the high anodic stability, enables a record high cycle life of >2,000 cycles for Li||LiFePO4 and >400 cycles for Li||LiCoO2 full cells.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.