Abstract

Bioactive hydroxyapatite (HA) coating on titanium (Ti) implant can be used as a drug delivery device. A controlled release of drug around the implant requires the incorporation of drug into the coating material during the coating process. HA coating was prepared using a two-step procedure in conditions suitable for simultaneous incorporation of the protein-based drug into the coating material. Monetite coating was deposited on Ti substrate in acidic condition followed by the transformation of the monetite coating to HA. X-ray diffraction (XRD) confirmed the formation of the monetite phase at the first step of the coating preparation, which was transformed into HA at the second step. Fourier transform infrared spectroscopy demonstrated typical bands of a crystallized carbonated HA with A- and B-type substitution, which was confirmed by the XRD refinement of the structural parameters. Scanning electron microscope was used to observe the morphology of monetite and HA coatings. Adhesion of the coatings was measured using a scratch tester. The critical shearing stress was found to be 84.20 ± 1.27 MPa for the monetite coating, and 44.40 ± 2.39 MPa for the HA coating.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.