Abstract

Non-metallic inclusions in API steel grades deteriorate steels’ mechanical properties and their resistance to hydrogen induced cracking. The formation and evolution of inclusion during liquid steel processing was investigated by analyzing samples taken from different stages of the steel making process in API X52 and X60 steel grades. Scanning electron microscope (SEM) with automated feature EDX analyzer (INCAF 250) was used to identify each inclusion in terms of its size, area and composition. It was found that non-metallic inclusions in API X52 and X60 grades from steelmaking and casting samples were mainly Al2O3, Ca–Al and Ca-Mg-Al. In this work changes in inclusion composition, size and area fraction from ladle processing to casting were mapped and this information was used to improve steel cleanness and product quality.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.