Abstract

The effect of using different reductors in the reduction process of nickel laterite was investigated. In this work, the author conducted the reduction of nickel laterite ores by anthracite coal, lamtoro charcoal, and carbon raiser, in air and CO2 atmosphere, within the temperature ranged from 800°C and 1000°C. The results indicate that at higher temperatures, the reduction reactions proceed more complete. According to the X-ray powder diffraction (XRD) analysis, the type of carbon used greatly influence the rate of the reduction of nickel laterite. The order of reactivity is anthracite coal, lamtoro charcoal, and carbon raiser, respectively. The reduction atmospheric condition also greatly influences the reduction process. The reduction process in CO2 atmospheric condition gives a lot of significant decrease in hematite and magnetite presence, means that the reduction reactions proceed more complete compared to the reduction process in the air atmospheric condition.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.