ABSTRACT This study investigated the physical, chemical, thermal, morphological, and XRD analysis of Symphirema involucratum stem fiber to establish its suitability in composite reinforcements. The investigation on chemical components proved that the fiber possesses a good amount of cellulose content (57.32%) with low lignin (13.85%), hemicellulose (12.47%), wax (0.56%), moisture (9.11%), and ash (9.05%) contents. The fiber showed a density of 1389 kg/m3, a diameter of 542.26 ± 10.32 µm, and a crystallinity index of 28.22%. Higher maximum degradation temperature (350°C) with a kinetic activation energy of 74.88 kJ/mol obtained by thermogravimetric analysis. Nuclear magnetic resonance spectra confirmed the presence of high cellulose content at the intensities of the C-2, C-3, and C-5 lines. The microscopic examination of the SISF through a scanning electron microscope and atomic force microscopy revealed that the fiber possesses quite a high coarse fracture surface with pores. The properties of the SISF propose its suitability toward use as an alternative to man-made synthetic fibers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.