Knowledge of accurate values of elastic modulus of (Al1-xScx)N is required for design of piezoelectric resonators and related devices. Thin films of (Al1-xScx)N across the entire composition space are deposited and characterized. Accuracy of modulus measurements is improved and quantified by removing the influence of substrate effects and by direct comparison of experimental results with density functional theory calculations. The 5%-30% Sc compositional range is of particular interest for piezoelectric applications and is covered at higher compositional resolution here than in previous work. The reduced elastic modulus is found to decrease by as much as 40% with increasing Sc concentration in the wurtzite phase according to both experimental and computational techniques, whereas Sc-rich rocksalt-structured films exhibit little variation in modulus with composition.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.