Abstract
Friction stir processing (FSP) is a novel technique used for the production of surface composite, refinement of microstructure and enhancing the mechanical properties. In this work, surface matrix composite (SMC) was fabricated on the surface of aluminium alloy (6063) with ceramic reinforcement using friction stir processing technique. SiC and Gr was used as reinforcement. The chosen FSP parameters such as traverse speed of 30mm/min, tool rotational speed of 1000rpm and 10 KN of axial load. The FSP tool made of HcHCr with cylindrical threaded profile pin having shoulder diameter of 18mm, pin length of 5.8mm and pin diameter of 6mm was used. The FSP was carried out using friction stir welding machine. Three combinations of surface composites (Al/0.8Vol.%SiC, Al/0.8Vol.%Gr and Al/0.4Vol.%SiC-0.4Vol.%Gr) were fabricated. Optical microscope (OM) and scanning electron microscope (SEM) was used to study the microstructural changes. The recrystallized grain structure was observed in the FSPed zone. The microhardness of friction stir processed plates was analyzed using a Vickers hardness tester. Sic reinforced Al alloy surface composite resulted higher microhardness.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: Procedia Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.