Abstract

The chitosan starch film was produce through solution casting with different carboxylic acid for acid treatment. Several testing were conducted such as tensile test, scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR), moisture absorption and soil burial. The optimum ratio for the chitosan/starch was 70:30. This ratio shows the highest tensile strength which is 11.84 MPa for the control film. The acid used for chemical modifications were citric acid and ascorbic acid. This acid modificationsexhibited higher tensile strength, Young's modulus, and less weight loss in soil burial and lower percentage of moisture absorption. SEM shows the better solubility of the starch in film with acid treatment. Moisture absorption and weight loss in the soil burial test was lower in the film with acid treatment than thefilm without acid treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.