Abstract

Preparing of cool wool from coarse wool fiber is a feasible and effective method. The preparation principle, process and properties of cool wool fiber was studied during chlorination treatment with sodium hypochlorite. The optimum chlorination treatment process was as follows: concentration of sodium hypochlorite at 4g/L, concentration of sulphuric acid at 20g/L, time 15min, temperature 20°C to 25°C, ratio of water and wool fiber was 50:1. Compared with original wool fiber,the surface of cool wool only retained scales roots and the cuticle becomes thinner. Handle, softness, whiteness, luster and the anti-shrinkage properties were improved, the breaking strength is decreased about 5% to 8%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.