Abstract

From decades it has been recognized that Geopolymer will considerably replace the role of cement in the construction industry. In general, Geopolymer exhibits the property of the peak compressive strength, minimal creep and shrinkage. In this current research paper, Geopolymer mortar is prepared by using GGBS and Fly ash. The mix proportions are of (100-60)%GGBS with Fly ash by 10% replacement. The alkali activators Na0H and Na2Sio3 are used in the study for two different molarities of 4&8. The ratio to Sodium silicates to sodium hydroxide is maintained from 1.5, 2, 2.5 & 3 were used. Mortars are prepared and studied the effect of molarities of alkali activators in their setting times and strengths.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.