Tricalcium phosphate (TCP) ceramics are useful biodegradable bone-repairing materials. Silicate-containing TCP ceramics are expected to be useful as biodegradable bone-repairing materials which promote the bone regeneration because it has been reported that the silicate promotes bone formation. In the present study, silicate-containing TCP ceramics were prepared through a wet chemical process at the starting compositions from 0 to 0.05 in the Si/(P+Si) molar ratio. The prepared silicate-containing TCP ceramics were characterized and evaluated in vitro. The crystal phase of the products was α-TCP, and the tendency that the lattice constants linearly shifted from 0 to 0.05 in the starting Si/(P+Si) molar ratio was observed. It is speculated that the added silicate was incorporated in the crystal structure of TCP. The pellets were prepared by a sintering process, and soaked in a simulated body fluid (SBF) to estimate their bone-bonding ability. The addition of silicate to TCP promoted to hydroxyapatite formation on the TCP ceramics in SBF. This result implies the high possibility that the silicate addition would promote the bone-bonding ability of the TCP ceramics.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.