This study analyzes thermal runaway (TR) characteristics via experiments conducted on lithium-ion batteries. To generate the TR of lithium-ion batteries, overcharge was applied as an electrical abuse condition. The TR experiment was conducted in a chamber with the dimensions of 1.5 × 1.5 × 1.5 m by classifying the capacity of a pouch-type lithium-ion battery and cathode material employed. The experimental results demonstrated that the lithium-ion battery before TR exhibited repetitive voltage and temperature characteristics, and that TR could be detected in advance based on these characteristics. TR occurred after the cell surface temperature of the lithium ion battery was maintained at approximately 100 ℃ for a certain duration. The voltage of the lithium-ion battery gradually increased before TR; however, the voltage decreased after the inflection point (Vmax) was crossed. Then, the voltage increased sharply after decreasing for a certain duration and was higher than the voltage increase rate (V/min) observed before the inflection point (Vmax) was attained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.